CAD/CAM lithium disilicate ceramic crowns: Effect of occlusal thickness on fracture resistance and fractographic analysis

Document Type

Article

Publication Title

Dental Materials Journal

Abstract

This study uses fracture tests and fractographical analysis to compare computer-aided design and computer-aided manufacturing (CAD/CAM) lithium disilicate molar crowns with the previous occlusal thickness recommendation of 1.5-mm, the new recommendation of 1.0-mm, and a less invasive thickness of 0.8-mm. After fatigue application, fracture tests and fractographic analysis were conducted. The fracture resistance of CAD/CAM lithium disilicate molar crowns was different depending on the occlusal thickness of the restoration, and decreased with lower the thickness. However, the fracture resistance of crowns of all three thicknesses exceeded the reported maximum bite force in the first molar region after the fatigue process, and can be considered acceptable for use in the clinic.

First Page

705

Last Page

709

DOI

10.4012/dmj.2022-018

Publication Date

1-1-2022

This document is currently not available here.

Share

COinS